Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 1.87 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.87 J/cm

@Temperature -40.0 °C
3.50 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Izod Impact, Notched 1.87 J/cm

@Temperature -40.0 °C
3.50 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Polymer Resources PPX-GP8 Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 240F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Izod Impact, Notched 1.87 J/cm

@Temperature 22.8 °C
3.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat
General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Izod Impact, Notched 1.87 J/cm

@Thickness 6.35 mm
3.50 ft-lb/in

@Thickness 0.250 in
ASTM D256
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 1.87 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
3.50 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM-D256
Ineos ABS Lustran® 750 ABS, Molding Grade
Lustran® 750 resin is a black, virgin injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is designed for molded drain, waste, and vent (DWV) fittings. Lustran® 750 (901802 bl..
Izod Impact, Notched 1.87 J/cm

@Temperature 23.0 °C
3.50 ft-lb/in

@Temperature 73.4 °F
3.2 mm (0.125 in) notch
Kraton® FG1901 + PA-6 blend (20/80)
Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A..
Izod Impact, Notched 1.87 J/cm

@Temperature 22.8 °C
3.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Teknor Apex Chemlon® 253 Nylon 6, Toughened
Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation ..
Izod Impact, Notched 1.87 J/cm

@Temperature 23.0 °C
3.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 105E3V36327 Acetate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Izod Impact, Notched 1.87 J/cm

@Temperature 23.0 °C
3.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Dow C702-20NA Polypropylene Impact Copolymer Resin
OverviewHigh impact performanceContains a nucleating additiveContains an antistatic additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C702-20NA Polypropylene Resin is intended f..
Copyright © lookpolymers.com All Rights Reserved