Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.87 J/cm @Temperature -40.0 °C |
3.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature -40.0 °C |
3.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PPX-GP8 Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 240F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 6.35 mm |
3.50 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.87 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
3.50 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM-D256 |
Ineos ABS Lustran® 750 ABS, Molding Grade Lustran® 750 resin is a black, virgin injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is designed for molded drain, waste, and vent (DWV) fittings. Lustran® 750 (901802 bl.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 23.0 °C |
3.50 ft-lb/in @Temperature 73.4 °F |
3.2 mm (0.125 in) notch |
Kraton® FG1901 + PA-6 blend (20/80) Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 22.8 °C |
3.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Chemlon® 253 Nylon 6, Toughened Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation .. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 23.0 °C |
3.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 105E3V36327 Acetate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Izod Impact, Notched | 1.87 J/cm @Temperature 23.0 °C |
3.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Dow C702-20NA Polypropylene Impact Copolymer Resin OverviewHigh impact performanceContains a nucleating additiveContains an antistatic additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C702-20NA Polypropylene Resin is intended f.. |