Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.721 J/cm @Temperature 0.000 °C |
1.35 ft-lb/in @Temperature 32.0 °F |
3.2 mm (0.125 in) notch |
Kraton® D1102 + PP blend (10/90) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Izod Impact, Notched | 0.720 J/cm @Temperature -40.0 °C |
1.35 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-665C30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |