Polymer Property : Izod Impact, Notched = 1.05 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.05 J/cm

@Temperature -40.0 °C
1.97 ft-lb/in

@Temperature -40.0 °F
ASTM D256
DuPont Performance Polymers Rynite® RE15022 NC010 PET  (Unverified Data**)
Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers
Izod Impact, Notched 1.05 J/cm

@Temperature -30.0 °C
1.97 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East)
XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid..
Izod Impact, Notched 1.05 J/cm

@Temperature -40.0 °C
1.97 ft-lb/in

@Temperature -40.0 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-669VGB Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.05 J/cm

@Temperature 23.0 °C
1.97 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Total PPC 4720XWZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 4720XWZ is a nucleated impact copolymer with a Melt Flow index of 25 g/10 min.TOTAL Polypropylene 4720XWZ is characterized by improved stiffness, creep resistance,..
Izod Impact, Notched 1.05 J/cm

@Temperature 23.0 °C
1.97 ft-lb/in

@Temperature 73.4 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.05 J/cm

@Temperature 23.0 °C
1.97 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Drystar 0325 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Izod Impact, Notched 1.05 J/cm

@Temperature 23.0 °C
1.97 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Drystar 0603 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Izod Impact, Notched 1.05 J/cm

@Temperature 23.0 °C
1.97 ft-lb/in

@Temperature 73.4 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-779 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..