Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.580 J/cm @Temperature -40.0 °C |
1.09 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar EN067 Copolyester, Natural Eastar Copolyester EN067 is a copolymer PET with good color. This product is supplied as a crystalline pellet that has improved flowability characteristics. Due to slower crystallization kinetics, t.. |