Polymer Property : Izod Impact, Notched = 0.430 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.430 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.806 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L0111 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 0.430 J/cm

@Temperature -40.0 °C
0.806 ft-lb/in

@Temperature -40.0 °F
ASTM D256
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)  (Unverified Data**)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Izod Impact, Notched 0.430 J/cm

@Temperature 23.0 °C
0.806 ft-lb/in

@Temperature 73.4 °F
DAM; ASTM D256
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612  (Unverified Data**)
Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.430 J/cm

@Temperature -30.0 °C
0.806 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66
NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe..
Izod Impact, Notched 0.430 J/cm

@Temperature 23.0 °C
0.806 ft-lb/in

@Temperature 73.4 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-808-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.430 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
0.806 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Diamond Polymers Centrex® 485 Sheet Extrusion Grade
Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it..
Izod Impact, Notched 0.430 J/cm

@Temperature 23.0 °C
0.806 ft-lb/in

@Temperature 73.4 °F
DAM; ASTM D256
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66
Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.430 J/cm

@Temperature 23.0 °C
0.806 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Braskem RP 145 RACO Random Polypropylene Copolymer
RP 145 is a high melt flow rate random copolymer designed for use in thin-walled injection molding parts. This product offers good transparency, very good stiffness/impact strength balance, excellen..