Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.210 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.393 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87707 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.210 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.393 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87717 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.210 J/cm @Temperature 23.0 °C |
0.393 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® INP576 ABS Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc.. |
|||
Izod Impact, Notched | 0.210 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
0.393 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Diamond Polymers Centrex® HGM Automotive Grade, Injection Molding Grade Centrex HGM resin is an exceptionally high-gloss grade of ASA (acrylonitrile-styrene-acrylate). This injection molding grade has excellent gloss retention, excellent resistance to chemicals and high.. |
|||
Izod Impact, Notched | 0.210 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.393 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L6180 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |