Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.130 J/cm @Temperature -30.0 °C |
0.244 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® INP576 ABS Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc.. |
|||
Izod Impact, Notched | 0.130 J/cm @Temperature -30.0 °C |
0.244 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® INP630 ABS INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance.
Provides excellent hi.. |
|||
Izod Impact, Notched | 0.130 J/cm @Thickness 4.00 mm, Temperature -20.0 °C |
0.244 ft-lb/in @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PP 1380 PRE-ELEC PP 1380 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity PR.. |