Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength | >= 22.0 g/25 mm | >= 0.0485 lb/in | using Tesa 7475 Tape |
DuPont Teijin Films Mylar® HR951 Polyester Film, 140 Gauge Mylar® HR951 is a one-side release coated polyester film with good handling properties and clarity. It has been developed for use in various industrial applications.Information provided by DuPont. |
|||
Heat Seal Strength | >= 22.0 g/25 mm | >= 0.0485 lb/in | Using Tesa 7475 Tape |
DuPont Teijin Films Mylar® RSX951 Polyester Film, 105 Gauge Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production.. |
|||
Heat Seal Strength | >= 22.0 g/25 mm | >= 0.0485 lb/in | Using Tesa 7475 Tape |
DuPont Teijin Films Mylar® RSX951 Polyester Film, 120 Gauge Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production.. |
|||
Heat Seal Strength | >= 22.0 g/25 mm | >= 0.0485 lb/in | Using Tesa 7475 Tape |
DuPont Teijin Films Mylar® RSX951 Polyester Film, 140 Gauge Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production.. |
|||
Heat Seal Strength | >= 22.0 g/25 mm | >= 0.0485 lb/in | Using Tesa 7475 Tape |
DuPont Teijin Films Mylar® RSX951 Polyester Film, 175 Gauge Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production.. |
|||
Heat Seal Strength | >= 22.0 g/25 mm | >= 0.0485 lb/in | Using Tesa 7475 Tape |
DuPont Teijin Films Mylar® RSX951 Polyester Film, 48 Gauge Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production.. |
|||
Heat Seal Strength | >= 22.0 g/25 mm | >= 0.0485 lb/in | Using Tesa 7475 Tape |
DuPont Teijin Films Mylar® RSX951 Polyester Film, 92 Gauge Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production.. |
|||
Heat Seal Strength | >= 22.0 g/25 mm | >= 0.0485 lb/in | using Tesa 7475 Tape |
DuPont Teijin Films Mylar® HR951 Polyester Film, 92 Gauge Mylar® HR951 is a one-side release coated polyester film with good handling properties and clarity. It has been developed for use in various industrial applications.Information provided by DuPont. |