Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Impact Test = 95.9 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 130 J
95.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East)
High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.