Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | >= 10.2 J | >= 7.50 ft-lb | GM 9751P |
Lord Adhesives Versilok® 253 / 254 Acrylic Adhesive LORD Versilok® 253/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum.. |
|||
Impact Test | >= 10.2 J | >= 7.50 ft-lb | GM 9751P |
Lord Adhesives Versilok® 262 / 254 Acrylic Adhesive LORD Versilok® 262/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Impact Test | >= 10.2 J | >= 7.50 ft-lb | GM 9751P |
Lord Adhesives Versilok® 262B / 254 Acrylic Adhesive LORD Versilok® 262B/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum.. |
|||
Impact Test | >= 10.2 J | >= 7.50 ft-lb | GM 9751P |
Lord Adhesives Versilok® 265 / 254 Acrylic Adhesive LORD Versilok® 265/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |