Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 33.9 - 56.9 J | 25.0 - 42.0 ft-lb | unnotched; Tempering: 3 x 1 h at 1040°F |
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel Chromium-molybdenum-tungsten-vanadium alloyed PM steelVanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications wh.. |