Impact Test 33.9 J

@Temperature 22.8 °C
25.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R21 ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.
Impact Test 33.9 J

@Temperature 22.8 °C
25.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R24 ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.
Impact Test 33.9 J

@Temperature 22.8 °C
25.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R71/920 PC/ABS Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
Impact Test 33.9 J

@Temperature 22.8 °C
25.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R922 PC/ABS Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
Impact Test 33.9 J

@Temperature 23.0 °C
25.0 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron CALIBREâ„¢ 7101 15 Polycarbonate, 10% Glass Reinforced
CALIBRE® 7101 is a 10% glass reinforced ignition resistant polycarbonate resin equipped with a mold release package for optimal processing. The CALIBRE 7101 resins exhibit a high modules, excepti..
Impact Test 33.9 J

@Temperature 23.0 °C
25.0 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 9035 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 33.9 - 56.9 J
25.0 - 42.0 ft-lb
unnotched; Tempering: 3 x 1 h at 1040°F
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel
Chromium-molybdenum-tungsten-vanadium alloyed PM steelVanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications wh..