Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Impact Test = 46.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 46.0 J

@Temperature 23.0 °C
33.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics Prevex BJAX PPE+PS
Foamable resin. All properties at 10% density reduction; 0.250" thick specimens; improved productivity.This data was supplied by SABIC-IP for the Americas region.
Impact Test 46.0 J

@Temperature 23.0 °C
33.9 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 275 ABS, Low Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 46.0 J

@Temperature 23.0 °C
33.9 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 8325 ABS, Sheet Coextrusion Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 46.0 J
33.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP)
LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s).
Copyright © lookpolymers.com All Rights Reserved