Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 46.0 J @Temperature 23.0 °C |
33.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Prevex BJAX PPE+PS Foamable resin. All properties at 10% density reduction; 0.250" thick specimens; improved productivity.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 46.0 J @Temperature 23.0 °C |
33.9 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Styron Magnum™ 275 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Impact Test | 46.0 J @Temperature 23.0 °C |
33.9 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Styron Magnum™ 8325 ABS, Sheet Coextrusion Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Impact Test | 46.0 J | 33.9 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP) LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s). |