Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 57.0 J @Temperature 23.0 °C |
42.0 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Impact Test | 56.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
42.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from.. |
|||
Impact Test | 56.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
42.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from.. |
|||
Impact Test | 56.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
42.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from.. |
|||
Impact Test | 56.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
42.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from.. |
|||
Impact Test | 56.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
42.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from.. |
|||
Impact Test | 57.0 J @Thickness 3.20 mm |
42.0 ft-lb @Thickness 0.126 in |
Instrumented Total Impact; 12.5 mm dart, 75 mm clamp, 6.7 m/s; ASTM D3763 |
Covestro Bayblend® FR 90 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
Impact Test | 57.0 J | 42.0 ft-lb | HRC 61, unnotched |
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel Vanadis 4 Extra is characterized by: Very good ductility High abrasive-adhesive wear resistance High compressive.. |
|||
Impact Test | 56.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
42.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman POLYAXIS® LP624 Stabilized High Density Polyethylene DescriptionPolyaxis CP 624 is a stabilized high density polyethylene rotational molding compound with good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from.. |
|||
Impact Test | 57.0 J @Thickness 3.20 mm |
42.0 ft-lb @Thickness 0.126 in |
Instrumented Total Impact; 3.2 mm thick, 12.5 mm dart, 75 mm clamp, 6.7 m/s; ASTM D3763 |
Covestro Bayblend® FR 90 Polycarbonate + ABS Blend, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |