Mechanical Properties Metric English Comments
Impact Test 49.0 J

@Temperature 23.0 °C
36.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp..
Impact Test 49.0 J
36.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC
LNP* LUBRICOMP* DL001 is a compound based on Polycarbonate resin containing 5% PTFE. Added features of this material include: Internally Lubricated.
Impact Test 49.0 J
36.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Asia Pacific)
LNP* Lubricomp* DL001 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated.
Impact Test 49.0 J

@Thickness 3.20 mm
36.1 ft-lb

@Thickness 0.126 in
Instrumented Total Impact; 3.2 mm thick, 12.5 mm dart, 75 mm clamp, 6.7 m/s; ASTM D3763
Covestro Bayblend® FR 2000 Polycarbonate/ABS Blend  (discontinued **)
Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin..
Impact Test 49.0 J

@Thickness 2.50 mm
36.1 ft-lb

@Thickness 0.0984 in
Instrumented Total Impact; 2.5 mm thick, 12.5 mm dart, 40 mm clamp, 3.3 m/s; ASTM D3763
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, Dry as Molded
Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi..
Impact Test 49.0 J
36.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP V1000SU PA
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.
Impact Test 49.0 J
36.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP V1000UXC PA
LNP* Thermotuf* V1000UXC is a compound based on Nylon resin. Added features of this material include: UV Stabilized.
Impact Test 49.0 J

@Temperature 23.0 °C
36.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl LS175 PPE+HIPS
Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del..
Impact Test 49.0 J

@Temperature 23.0 °C
36.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl LS175 PPE+HIPS (Europe-Africa-Middle East)
Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del..
Impact Test 49.0 J
36.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOTUF VX99809 Super Tough Nylon
Super Tough Nylon, Proprietary Filler(s),