Polymer Property : Impact Test = 30.2 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 41.0 J

@Thickness 2.50 mm
30.2 ft-lb

@Thickness 0.0984 in
Instrumented Impact, Total Energy; 2.5 mm thick, 7.6 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
Covestro Bayblend® 2153 Polycarbonate + ABS Blend, General Purpose  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Impact Test 41.0 J

@Thickness 2.50 mm
30.2 ft-lb

@Thickness 0.0984 in
Instrumented Impact, Total Energy; 7.6 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
Covestro Bayblend® 2753 Polycarbonate + ABS Blend, Automotive  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Impact Test 41.0 J

@Temperature 23.0 °C
30.2 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics LNP Lubricomp TX03476 PU
LNP* Lubricomp* TX03476 is a Polyurethane containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region.
Impact Test 41.0 J
30.2 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON TX06488NTX1 PU
LNP* STAT-KON* TX06488NTX1 is a compound based on Polyurethane resin containing Proprietary Filler(s). Added features of this grade are: Execllent Ductility, Electrically Conductive.