Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 3.95 J | 2.91 ft-lb | ASTM D2794 |
3M Scotchkote™ HB 850 Epoxy Floor Coating Scotchkote Epoxy Floor Coating HB 850 has been specifically developed as a 100% solids protection system for application to a wide rage of floor surfaces.Product Features:Combines good application c.. |