Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchkote™ HB 850 Epoxy Floor Coating

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ HB 850 Epoxy Floor Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Epoxy Floor Coating HB 850 has been specifically developed as a 100% solids protection system for application to a wide rage of floor surfaces.Product Features:Combines good application characteristic with excellent chemical resistanceDesigned for application by brush or rollerSuitable for use on most floor surfaces in conjunction with the appropriate primer Information provided by 3M
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
Solids Content 100 %
100 %
Thickness 203 microns
8.00 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.7 MPa
2280 psi
ASTM D638
Impact Test 3.95 J
2.91 ft-lb
ASTM D2794
Abrasion 20
20
[mg] per 1000 cycles, 1 kg, CS17 Wheel; ASTM D4060
Processing Properties Metric English Comments
Cure Time 360 min
6.00 hour
Touch Dry
1440 min
24.0 hour
Hard Dry
10100 min
168 hour
Full Cure
Descriptive Properties Value Comments
Appearance Light Gray, Mid Gray, Dark Gray, Stone, Red, Mid Green
Users viewing this material also viewed the following: