Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 29.7 J @Thickness 3.17 mm |
21.9 ft-lb @Thickness 0.125 in |
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763 |
Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: BK15 is an SBC consisting of our developmental BK10 grade with a mold release added for easier processing. BK15 molded parts give excellent detail on f.. |
|||
Impact Test | 29.7 J @Thickness 3.17 mm |
21.9 ft-lb @Thickness 0.125 in |
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763 |
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding. Molded parts provide excellent part detail on fast production cycles. Molded parts have excellent c.. |
|||
Impact Test | 29.7 J @Thickness 3.17 mm |
21.9 ft-lb @Thickness 0.125 in |
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763 |
Chevron Phillips K-Resin® BK10 Styrene-Butadiene Copolymer, Injection Molding Grade Styrene-Butadiene CopolymerCustomer Benefits: BK10 is an SBC developed specifically to have enhanced flow capabilities. It offers improved processability and lower cycle times with the optical clar.. |
|||
Impact Test | 29.7 J @Thickness 3.17 mm |
21.9 ft-lb @Thickness 0.125 in |
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763 |
Chevron Phillips K-Resin® KR03 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give excellent part detail on fast production cycles. It can be t.. |
|||
Impact Test | 29.7 J @Thickness 3.17 mm |
21.9 ft-lb @Thickness 0.125 in |
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763 |
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR03 to facilitate printing.Customer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give .. |
|||
Impact Test | 29.7 J @Thickness 3.17 mm |
21.9 ft-lb @Thickness 0.125 in |
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763 |
Chevron Phillips K-Resin® KR05 Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Finished products have excellent clarity, good toughness, good s.. |
|||
Impact Test | 29.7 J @Thickness 3.17 mm |
21.9 ft-lb @Thickness 0.125 in |
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763 |
Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR05 to facilitate printing.Customer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Fin.. |
|||
Impact Test | 29.7 J @Thickness 3.17 mm |
21.9 ft-lb @Thickness 0.125 in |
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763 |
Chevron Phillips K-Resin® BK11 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: BK11 is an SBC consisting of KR03 grade with a mold release added of easier processing. BK11 molded parts give excellent detail on fast production cycl.. |