Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 27.0 J @Temperature 0.000 °C |
19.9 ft-lb @Temperature 32.0 °F |
multiaxial, 15 mph; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 2325 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2325 engineered polyolefin is designed for mold-in-color automotive interior applications. This material exhibits excellent low-gloss surface appearance and processability. Ap.. |
|||
Impact Test | 27.0 J @Temperature 0.000 °C |
19.9 ft-lb @Temperature 32.0 °F |
multiaxial, 15 mph; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 2382 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2382 engineered polyolefin is designed for large mold-in-color interior applications that require stiffness and dimensional stability. This material exhibits excellent process.. |
|||
Impact Test | 27.0 J @Temperature -29.0 °C |
19.9 ft-lb @Temperature -20.2 °F |
Montell drop weight impact strength |
LyondellBasell Pro-fax SB787 Polypropylene Impact Copolymer Key Features: blush resistance, excellent dimensional satiability, fast cycling, easy molding, good cold impact resistance, good stiffness and impact balance, easily colored, FDA acceptableApplicati.. |
|||
Impact Test | 27.0 J @Temperature 23.0 °C |
19.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas .. |
|||
Impact Test | 27.0 J | 19.9 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DX00887C PC LNP STAT-KON* DX00887C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Impact Test | 27.0 J | 19.9 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable. |
|||
Impact Test | 27.0 J | 19.9 ft-lb | ASTM D3763 |
ExxonMobil Exxtral™ H1025 Performance Polyolefin Product Description: A specialty thermoplastic olefin resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for automotive exterior applications.Availability.. |
|||
Impact Test | >= 27.0 J @Temperature -40.0 °C |
>= 19.9 ft-lb @Temperature -40.0 °F |
from AM 611; EN 10045-1 |
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |