Material Notes:
Key Features: blush resistance, excellent dimensional satiability, fast cycling, easy molding, good cold impact resistance, good stiffness and impact balance, easily colored, FDA acceptableApplications: automotive parts, housewares, closures, molds that are hard to fill, large or heavy partsMeets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.Description: Pro-fax SB787 easy molding, blush-resistant, medium impact polypropylene copolymer resin is available in pellet form. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. It has a UL yellow card RTI, which applies to all colors.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 230 °C
22 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256A
Impact Test 27.0 J

@Temperature -29.0 °C
19.9 ft-lb

@Temperature -20.2 °F
Montell drop weight impact strength
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
ASTM D648
UL RTI, Mechanical with Impact 115 °C
239 °F
Minimum thickness 0.037 inches.
Flammability, UL94 HB
HB
Minimum thickness 0.037 inches.