Mechanical Properties Metric English Comments
Impact Test 22.6 - 33.9 J
16.7 - 25.0 ft-lb
Torque Break
Ritelok TL71 Stud & Bolt Threadlocker
Anaerobic. High strength threadlocker for nuts, bolts, and heavy duty fasteners. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant
Impact Test 22.6 - 33.9 J
16.7 - 25.0 ft-lb
Prevail
ND Industries StudGrade® 137 Permanent HT Threadlocker
General DescriptionHigh strength, high temperature threadlockers for heavy duty applications. Suitable for most applications where disassembly is not required.
Impact Test 22.6 - 33.9 J
16.7 - 25.0 ft-lb
Break
ND Industries StudGrade® 140 Permanent Threadlocker
General DescriptionHigh strength threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical Usesstuds and bolts, and threaded pipe fittings.Meets m..
Impact Test 22.6 - 33.9 J
16.7 - 25.0 ft-lb
Prevail
ND Industries StudGrade® 146 Permanent StudGrade HD Threadlocker
General DescriptionHigh strength, high viscosity threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical UsesFasteners over 1" diameter with coa..