Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 29.0 J @Temperature -29.0 °C |
21.4 ft-lb @Temperature -20.2 °F |
Montell drop weight impact strength |
LyondellBasell Pro-fax 7823 Polypropylene Impact Copolymer, Fractional Melt Flow Key Features: high extrudate melt strength, good cold impact resistance, good stiffness and impact balance, FDA acceptableApplications: pipe, tubing, sheet, profiles, netting, blown containers and i.. |
|||
Impact Test | 29.0 J @Temperature -29.0 °C |
21.4 ft-lb @Temperature -20.2 °F |
Montell drop weight impact strength |
LyondellBasell Pro-fax SB786 Polypropylene Impact Copolymer Key Features: blush-resistant, easy molding, high impact polypropylene copolymer resin, good cold impact resistance, good stiffness, FDA acceptableApplications: automotive battery case, housewares, .. |
|||
Impact Test | 29.0 J | 21.4 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Impact Test | 29.0 J | 21.4 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific) LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Impact Test | 29.0 J | 21.4 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque. |
|||
Impact Test | 29.0 J @Thickness 4.00 mm |
21.4 ft-lb @Thickness 0.157 in |
Multi-axial, at failure; ASTM D3763 |
Azdel AZMET® CM20350 35% continuous random fiber mat / PBT resin matrix AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polybutylene Terephthalate (PBT) resin matrix. This composite material fea.. |
|||
Impact Test | 29.0 J @Temperature -30.0 °C |
21.4 ft-lb @Temperature -22.0 °F |
Dynatup Impact, E at Max Load, Ductile; ASTM D3763 |
LyondellBasell Hifax™ ETA-3131 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus thermoplastic olefin resin, excellent impact and stiffness balance, excellent processabilityApplications: automotive filler and valance panels, lower a.. |