Impact Test 3.29 J
2.43 ft-lb
Multi-Axial Instrumented Impact Energy; ISO 6603-2
LNP Thermocomp® STN-F-1006 HS Polyamide 46, Glass Fiber Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..