Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 23.0 J | 17.0 ft-lb | multiaxial, 15 mph; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 2380 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2380 engineered polyolefin is designed for large mold-in-color automotive interior applications that require stiffness and dimensional stability over a broad temperature range... |
|||
Impact Test | 23.0 J | 17.0 ft-lb | Instrumented Impact Total Energy; ASTM D3763 |
ExxonMobil LD 051.LJ Molding, Extrusion and Compounding Resin
(discontinued **) LD 051.LJ resin is used in Blow molded, squeeze bottles, Pail lids, Closures, and Extruded profiles.Information provided by ExxonMobil Chemical |
|||
Impact Test | 23.0 J | 17.0 ft-lb | Instrumented Impact Total Energy; ASTM D3763 |
ExxonMobil LD 641.LN Molding, Extrusion and Compounding Resin
(discontinued **) LD 641.LN is a low density homopolymer specifically designed for high performance blow molding applications. This resin is suitable for applications requiring high melt strength, flexibility, good .. |
|||
Impact Test | 23.0 J @Temperature -29.0 °C |
17.0 ft-lb @Temperature -20.2 °F |
Montell drop weight impact strength |
LyondellBasell Pro-fax SB891 Polypropylene Impact Copolymer Key Features: high flow, compatible with hindered amine light stabilizers, good cold impact resistance, good stiffness and impact balance, high flow for ease of mold filling and minimum warpageAppli.. |
|||
Impact Test | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
Multi-axial Impact; ASTM D3763 |
Flint Hills AP7710-HS Impact Copolymer Polypropylene TPO copolymer, UL certified, and FDA compliant.Features: Structural stiffness, ultra high impact strength, and high uniform flow rate.Applications: Injection molding: automotive items and exterior e.. |
|||
Impact Test | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
MAII, E at Max Load, Ductile; ISO 6603-2 |
LyondellBasell Hifaxâ„¢ CB228 Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good paintability, good processabilityApplications: aut.. |
|||
Impact Test | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
MAII, E at Max Load, Ductile; ISO 6603-2 |
LyondellBasell Hifaxâ„¢ CJ232 Thermoplastic Olefin Resin Key Features: medium high melt flow, medium modulus, low CLTE, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good dimensional stability, paintableApplicat.. |
|||
Impact Test | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon TE002 LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Impact Test | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Impact Test | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Impact Test | 23.0 J | 17.0 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp DF002L PC LNP THERMOCOMP* DF002L is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC-IP for the America.. |
|||
Impact Test | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
Dynatup Impact, E at Max Load, Ductile; ASTM D3763 |
LyondellBasell Hifax™ CB235 Thermoplastic Olefin Resin Key Features: medium high melt flow, medium high modulus, paintable thermoplastic olefin resin, excellent impact and stiffness balance, good dimensional stability, excellent processability, good pai.. |
|||
Impact Test | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
Dynatup Impact, E at Max Load, Ductile; ASTM D3763 |
LyondellBasell Hifax™ ETA-3183EN Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, paintable thermoplastic olefin resin, excellent impact and stiffness balance, good dimensional stability, good paintability, good processabilityA.. |