Polymer Property : Impact Test = 15.8 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 15.8 J

@Thickness 3.17 mm
11.7 ft-lb

@Thickness 0.125 in
Drop Impact, plaques. Fina API test
Total PPR 7525MZ Polypropylene, Injection Molding Grade
Clarified random copolymer for injection moldingClarity - FINA 7525MZ exhibits superior clarity in molded parts.Impact - FINA 7525MZ produces molded parts with improved impact compared with parts mo..