Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 15.8 J @Thickness 3.17 mm |
11.7 ft-lb @Thickness 0.125 in |
Drop Impact, plaques. Fina API test |
Total PPR 7525MZ Polypropylene, Injection Molding Grade Clarified random copolymer for injection moldingClarity - FINA 7525MZ exhibits superior clarity in molded parts.Impact - FINA 7525MZ produces molded parts with improved impact compared with parts mo.. |