Impact Test 20.5 J
15.1 ft-lb
multiaxial, at 2.2 m/sec, 100% ductile; ASTM 3763
S&E Specialty Polymers TufFillâ„¢ 5004UV Polyolefin
Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p..