S&E Specialty Polymers TufFill™ 5004UV Polyolefin

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer S&E Specialty Polymers
Trade Name TufFill™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufFill™ 5004UV Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV protection or paintable version.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
ISO 1183
Melt Flow 38.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
38.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength 18.0 MPa
2610 psi
ISO 527
Flexural Modulus 1.577 GPa
228.7 ksi
ISO 178
Izod Impact, Notched (ISO) 8.30 kJ/m²

@Temperature -30.0 °C
3.95 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
NB

@Temperature 24.0 °C
NB

@Temperature 75.2 °F
ISO 180/1A
Impact Test 20.5 J
15.1 ft-lb
multiaxial, at 2.2 m/sec, 100% ductile; ASTM 3763
Multi-axial Impact @ -30°C Total Energy 23.8 J
17.6 ft-lb
ASTM 3763; at 2.2 m/sec, 100% ductile