Polymer Property : Impact Test = 13.6 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 13.6 J
10.0 ft-lb
Reverse; ASTM D2794
Chesterton ARC MXHT High temperature severe wear compound
Description: An advanced ceramic composite for the protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack at elevated temperatures. It is applied at a thickness o..