Mechanical Properties Metric English Comments
Impact Test 17.6 J
13.0 ft-lb
@ -4ºF, Instrumented Impact Total Energy; ASTM D3763
ExxonMobil LD 516.LN Molding, Extrusion and Compounding Resin
Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un..