Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 2.65 J | 1.95 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Lubricomp® EFL-4034 LE BK8-065 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued ** Features: Low Extractables, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Impact Test | 2.64 J | 1.95 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Thermocomp® EF-1006 BK8-114 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |