Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 2.41 J | 1.78 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Stat-Kon® PDX-E-99689 CCS Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued.. |