Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 1.48 J | 1.09 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Lubricomp® EL-4030 Polyetherimide, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Impact Test | 1.48 J | 1.09 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |