Polymer Property : Toughness = 73.8 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Toughness 100 J
73.8 ft-lb
Per square meter; ASTM D399
Hexcel® HexPly® 171/174/176 120°C Curing Epoxy Matrix
The HexPly® 174 family is a range of flexible 120°C curing matrix systems for a wide variety of industrial applications and is ideally matched to the following processes: shrink wrap tape, vacuum ..