Material Notes:
The HexPly® 174 family is a range of flexible 120°C curing matrix systems for a wide variety of industrial applications and is ideally matched to the following processes: shrink wrap tape, vacuum bag, press or autoclave manufacturing methods. HexPly® 174 comprises a modified epoxy resin pre-impregnated into carbon, glass or aramid fibers, It cures at 120°C to form a tough durable fiber-reinforced composite.Three versions of HexPly® 174 are available:HexPly® 171 - fabric reinforcementHexPly® 174 - UD tape and single tow reinforcementHexPly® 176 - fabric reinforcement, improved surface finishInformation provided by HexCel
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1675-1975
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO R527
Elongation at Yield 2.6 %
2.6 %
ISO R527
Tensile Modulus 2.80 GPa
406 ksi
ISO R527
Toughness 100 J
73.8 ft-lb
Per square meter; ASTM D399
Thermal Properties Metric English Comments
CTE, linear 67.0 µm/m-°C
37.2 µin/in-°F
Glass Transition Temp, Tg 110 - 120 °C
230 - 248 °F
DAN 432
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F