Polymer Property : Toughness = 140 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Toughness 190 J
140 ft-lb
Per square meter
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix
HexPly® M36 is a high performance 180ºC cure matrix developed for aerospace and industrial markets. It can be used in a variety of production techniques (Resin Film Infusion (RFI), prepreg and sem..