Mechanical Properties Metric English Comments
300% Modulus 0.0380 GPa
5.51 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1180H Super Hard Polyester Based TPU
Low mold shrinkage, good impact resistance, perfect transparency, good mold release, fatigue resistance, chemical & hydrolytic resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0380 GPa
5.51 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR5520 Standard Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..