Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.02748 GPa | 3.985 ksi | Formulation Example |
TSE Industries Millathane® 66 Millable Polyurethane Rubber Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical .. |
|||
300% Modulus | 0.02748 GPa | 3.985 ksi | Formulation Example |