Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 66 Millable Polyurethane Rubber

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 66 Millable Polyurethane Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical strength.Example FormulationMillathane 66 100.0Stearic Acid 0.25StabaxolP3.0N330 Black 20.0Di-Cup 40 C6.5TAC1.0All information provided by TSE Industries
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
approximately
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
Formulation Example
Tensile Strength, Yield 28.99 MPa
4205 psi
Formulation Example
Elongation at Yield 310 %
310 %
Formulation Example
100% Modulus 0.00380 GPa
0.551 ksi
Formulation Example
200% Modulus 0.01231 GPa
1.785 ksi
300% Modulus 0.02748 GPa
3.985 ksi
Formulation Example
Tear Strength 37.0 kN/m
211 pli
Formulation Example
Compression Set 11 %

@Temperature 100 °C,
Time 79200 sec
11 %

@Temperature 212 °F,
Time 22.0 hour
Formulation Example
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
under dry and cool conditions
Descriptive Properties Value Comments
Appearance White to amber solid bale or milled sheets