300% Modulus 0.0259 GPa
3.76 ksi
Dow Pellethane® 2354-65D Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2354-65D elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyurethane..