Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Pellethane® 2354-65D Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Pellethane® 2354-65D Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PELLETHANE® 2354-65D elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyurethane and acrylic enamels or water based elastomeric paints without a primer.Data provided by Dow Chemical.This product is no longer a part of the PELLETHANE® product line.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Melt Flow 24 g/10 min

@Load 5.00 kg,
Temperature 224 °C
24 g/10 min

@Load 11.0 lb,
Temperature 435 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Tensile Strength at Break 40.0 MPa
5800 psi
Tensile stress at break.
Elongation at Break 430 %
430 %
50% Modulus 0.0165 GPa
2.39 ksi
100% Modulus 0.0193 GPa
2.80 ksi
300% Modulus 0.0259 GPa
3.76 ksi
Tear Strength 210 kN/m
1200 pli
Taber Abrasion, mg/1000 Cycles 40
40
H22 Wheel
Compression Set 25 %
25 %
23°C.
25 %

@Temperature 70.0 °C
25 %

@Temperature 158 °F
Thermal Properties Metric English Comments
CTE, linear 117 µm/m-°C

@Temperature 20.0 °C
65.0 µin/in-°F

@Temperature 68.0 °F
Vicat Softening Point 141 °C
286 °F
Clash Berg Stiffness Temperature -17.8 °C
-0.0400 °F
Copyright © lookpolymers.com All Rights Reserved