300% Modulus 0.0180 GPa
2.61 ksi
DIN 53504
Huntsman IROGRAN® A 92 K 5031 TPU-High Temperature Performance
Polycaprolactone and ether based. Good processability and compression set. Excellent resistance to high temperatures, water, grease, and oils.. Used in seals, wheels, and rollers.Information prov..
300% Modulus 0.0180 GPa
2.61 ksi
ISO 37
Huntsman AVALON® 95 AE Thermoplastic Polyurethane
Introduction: AVALON 95 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AE is part of the AVALON Perform Range and offers a premium soiling materi..
300% Modulus 0.0180 GPa
2.61 ksi
ISO 37
Huntsman AVALON® 95 AEU Thermoplastic Polyurethane
Introduction: AVALON 95 AEU is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AEU is part of the AVALON Perform Range and offers a premium soiling mate..
300% Modulus 0.0180 GPa
2.61 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1695AB Polyester Based TPU
Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd.