Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wanhua Chemical Wanthane® WHT-1695AB Polyester Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-1695AB Polyester Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength 42.0 MPa
6090 psi
ASTM D412
Elongation at Break 460 %
460 %
ASTM D412
100% Modulus 0.00900 GPa
1.31 ksi
ASTM D412
300% Modulus 0.0180 GPa
2.61 ksi
ASTM D412
Tear Strength 122 kN/m
696 pli
ASTM D624
Abrasion 122
122
Abrasion resistance, mm<sup>3</sup>; ISO 4649
Processing Properties Metric English Comments
Processing Temperature 190 - 210 °C
374 - 410 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved