Polymer Property : 300% Modulus = 2.41 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0166 GPa
2.41 ksi
DIN 53504
Huntsman IROGRAN® A 92 P 4207 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman