Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0166 GPa | 2.41 ksi | DIN 53504 |
Huntsman IROGRAN® A 92 P 4207 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |