Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00869 GPa | 1.26 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.00869 GPa | 1.26 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 25 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.00870 GPa | 1.26 ksi | DIN 53504 |
Huntsman IROGRAN® A 80 P 5039 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
300% Modulus | 0.00869 GPa | 1.26 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.00869 GPa | 1.26 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 25 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |