Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 25 PHR Tricresyl Phosphate

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 25 PHR Tricresyl Phosphate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is carried out by the use of various peroxides including dicumyl peroxide (DCP) or 2,5-dimethyl-2,5-bis (t-butylperoxy) hexane (DBPH).FormulationMillathane 5004100Stearic Acid0.25N330 (HAF) Black20Di-Cup 40C5Tricresyl Phosphate25All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
Tensile Strength, Yield 23.0 MPa
3330 psi
Elongation at Yield 530 %
530 %
300% Modulus 0.00869 GPa
1.26 ksi
Tear Strength 84.1 kN/m
480 pli
ASTM Die C
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 152 °C
1.00 hour

@Temperature 305 °F